Magnetic Particle Inspection of Castings and Forgings Across the United States

Magnetic particle inspection of castings and forgings finds surface and near-surface flaws such as cracks, laps, seams, hot tears and shrinkage that break the surface of steel valve bodies, flanges, fittings, shafts, gears and hooks. Atlantis NDT mobilizes technicians to foundries, forge shops, machine shops, receiving docks and plants in the United States to examine to ASTM E1444, ASTM A275 and MSS SP-53 requirements and report every indication. To get started, request a castings and forgings MPI quote.

Why castings and forgings need their own technique

A weld is a thin, linear target; a casting or forging is a complex shape with thick sections, sudden changes in cross section, fillets, bores and parting lines. The flaws are different too. Castings can carry shrinkage cavities and hot tears where metal solidified unevenly, cold shuts where two streams failed to fuse, and surface porosity from gas. Forgings can carry laps and folds where metal was folded over during forming, seams inherited from the billet, quench cracks and grinding cracks introduced after heat treatment. Magnetic particle testing shows surface-opening versions of all of these on ferromagnetic carbon, low-alloy and martensitic stainless steel.

Because geometry strongly influences how a magnetic field travels, a procedure for one part rarely suits another. The technique is set by part shape, size and surface finish, not just by material.

Standards that apply

US purchase specifications, valve standards and construction codes reference a small group of documents for this work:

Acceptance levels come from the purchase order, the valve or flange specification and the end-use code. We apply the one named in your documents and do not choose a level ourselves.

Bench units, portable yokes and part-specific magnetizing

Shop work on small and mid-size parts is usually done on a stationary wet horizontal bench, where the part is clamped between heads and current passes through it for circular magnetization while a coil adds longitudinal magnetization. Atlantis technicians often work at your site and so more commonly use portable equipment: yokes, portable coils and cable wraps. The right choice depends on size, weight and where the part sits.

Receiving inspection and incoming material checks

Many orders for this work are receiving inspections. A purchaser takes delivery of valve castings, forged flanges or a batch of hooks and wants a sample or full examination before the parts are machined, assembled or welded into a system. Finding a cast or forging defect at the receiving dock is much cheaper than finding it after machining has added value. We can examine at your receiving area, plant floor or laydown yard, mark rejected pieces, and report each lot. Where specification allows sampling, the sampling plan comes from your purchase order, not from us.

Weld repairs of castings are a special case. A foundry may grind out a defect and weld the cavity; MT of the excavation before welding, and again after finishing, confirms the repair is sound. Weld-specific technique is covered on our magnetic particle weld inspection page.

Typical flaws and the method that finds them
FlawMTPTUT
Surface-open crack, lap or seam in carbon steel forgingStrongWorksPoor for surface flaws
Hot tear or surface shrinkage on a castingStrong where magneticWorksSubsurface part only
Internal shrinkage cavityWeakNoStrong
Flaw in austenitic stainless castingNoFirst choiceLimited by grain structure
Wall thickness of a valve bodyNoNoYes

Our penetrant testing and ultrasonic testing services cover the cases where MT is not the right tool, and the complete guide to magnetic particle testing explains the theory.

Surface preparation on cast and forged surfaces

As-cast surfaces are rough, scaled and sometimes sand-coated, and as-forged surfaces carry scale and tool marks. Rough surfaces trap particles and create non-relevant indications that look like cracks. The procedure states whether the surface must be blasted, ground or machined before examination and what finish is acceptable. Painted or primed parts need coating removed or limited to the thickness the procedure permits. We discuss surface condition before mobilization so the examination happens on parts that are ready.

Non-relevant indications on these parts are common: magnetic writing where parts touched, flux concentration at keyways and sharp section changes, and changes of permeability at weld repairs or heat-treated zones. A trained technician tells these from true flaws by re-magnetizing, re-cleaning and re-examining, and the report states what was done.

What the report contains

Heat treatment, grinding and machining: when to examine

The point in the manufacturing route where MT is performed decides which flaws it can catch. Specifications for forgings usually require examination after heat treatment and rough machining, since quench cracks form during cooling and are most visible on a machined surface. Grinding cracks appear after final grinding of hardened parts such as gears and shafts, and a procedure that calls for a post-grind examination catches them before assembly. Castings are typically examined after cleaning and after any weld repair, and again after final machining on critical surfaces such as valve seats and sealing faces.

Purchasers who inspect only at receiving may miss flaws that machining later removes or exposes, so an examination plan that ties MT to named process points gives a clearer record. If you are unsure where the examination belongs, send us the route sheet and the specification, and we will propose hold points for your quality lead to approve. The final plan remains your decision, since it reflects your own customer's requirements.

Identification and traceability

Each examined piece should be traceable back to its heat or lot. We record the heat number, part number and serial marking where present, and we mark the part with an accepted method only if your specification allows. Low-stress stamping and etching are often restricted on pressure-retaining parts, so we use paint pens, tags or sketches where marking could harm the part. Rejected pieces are segregated by your staff according to your nonconformance procedure.

What to send for a quote

Planning realities

Foundries and forge shops are hot, dusty and noisy, and parts may still be warm from heat treatment. Tell us the part temperature, since wet particles have temperature limits and dry powder tolerates more heat. Heavy parts need cranes or lift tables from your site, and fluorescent work requires a dark area that is often hard to find on a busy plant floor. We travel to your site with portable equipment; Atlantis has no office near it, so you should plan power, lighting and part staging as part of the scope.

Where we work in the United States

See also industry pages for automotive, steel, oilfield, mining, rail and power, and the national magnetic particle testing page.

Training your own technicians

If a plant examines parts every day, in-house staff may be cheaper. Atlantis provides MT Level 1 training and MT Level 2 training aligned to SNT-TC-1A, with practice in the magnetic particle simulator. Under SNT-TC-1A the plant, not the course provider, issues the certification.

What we do not do here

Atlantis does not perform radiography in the United States, and it does not judge casting soundness for service beyond reporting indications against your criteria. Internal shrinkage and porosity deeper than the surface layer need other techniques, including ultrasonic testing where the part geometry allows. Our scope here stops at the three methods named on this page.

Frequently asked questions

What does MT find in castings that visual inspection misses?

Tight surface cracks, hot tears, cold shuts and shallow subsurface flaws that are too fine or too dirty to see. The particles gather along the flaw and make it visible, even when the crack is only a few thousandths of an inch wide.

Which standard governs magnetic particle examination of forgings?

ASTM A275, adopted by ASME as SA-275, describes the examination of steel forgings. The purchase order or product specification sets acceptance levels, and ASTM E1444 and E709 support the technique.

What is MSS SP-53 used for?

MSS SP-53 describes magnetic particle examination of steel castings and forgings for valves, flanges, fittings and similar components. It is cited in valve and piping component specifications, which set the acceptance criteria.

What are ASTM E125 reference photographs?

E125 is a set of reference photographs showing typical magnetic particle indications on ferrous castings. Specifications that cite it let the examiner classify indications by comparing them with the photographs.

Can you inspect austenitic stainless steel castings with MT?

No, because austenitic stainless is not magnetic. Liquid penetrant testing is the normal surface method for those castings, and ultrasonic testing may be used for volume flaws where the grain structure allows.

Do you inspect on a bench or on site?

We usually work at your site with portable yokes, coils and cable wraps. If you have a stationary bench unit and need it operated, tell us when you request a quote so we can scope the work and write the procedure.

What is the difference between head shot and coil shot?

A head shot passes current through the part, giving a circular field that finds longitudinal cracks. A coil shot places the part in a coil, giving a longitudinal field that finds transverse cracks. Many parts need both.

Can MT be performed on hot parts?

Within limits. Wet particle suspensions have temperature ceilings and dry powder tolerates more heat, so the procedure states the allowed range. Tell us the part temperature and we will check it against the procedure before mobilizing.

Who decides whether a casting is accepted?

The purchaser, the specification or the engineer of record. We apply the acceptance criteria in your purchase order and report each indication with its location and size, so the decision maker has the facts.

Do you do sampling inspection of incoming lots?

Yes, if your purchase order or quality plan defines the sampling. We follow the plan you give us and report each part examined, including rejected pieces and the lot status your plan requires.

Related MT inspection pages

MT inspection by US city: Detroit, MI · Pittsburgh, PA · Milwaukee, WI · Birmingham, AL · Houston, TX · Cleveland, OH · Peoria, IL · Fort Wayne, IN.

Training your own technicians: MT Level 1 training · MT Level 2 training · MT practice simulator.

Request a MT inspection quote

Tell us about the magnetic particle inspection of castings and forgings work: the components and material, the quantity or weld list, the code or specification, access and temperatures, and the site address in the United States. We reply within one business day with the scope, the procedure we would use and the next step.

Request a MT inspection quote

Need magnetic particle testing (MT) done, or learned?

Atlantis provides magnetic particle testing (MT) as an inspection service, trains technicians in it, and lets teams practise it on the Practical NDT simulator.