Magnetic Particle Inspection (MT) in Spokane, Washington
Atlantis NDT provides magnetic particle inspection in Spokane, Washington, for steel weldments, crane and lifting components, structural steel and machinery parts. Technicians travel to your plant, yard or fabrication shop with yokes, particles and lighting, examine ferromagnetic surfaces to a written procedure, and report each indication against the acceptance criteria you specify. Send the part or weld list through the Spokane MT inspection quote request and we reply within one business day.
Where magnetic particle inspection earns its keep in Spokane
Spokane has a long history of working steel. Fabrication shops build structural frames, tanks, platforms and machinery, and the aluminum and metals plants in the Spokane Valley depend on cranes, casting machinery and heavy handling equipment made largely of carbon steel. Freight rail corridors cross the region, and bridges carry highways and local roads over the Spokane River and its gorge. All of that steel carries welds, and welds crack where stress concentrates: at toes, at attachment points, at lifting lugs and at repairs made in the field.
The components that most often come up on an MT work list in a city like this are easy to name. Overhead crane hooks, lifting beams, shackles, sheave pins and trunnions are examined for fatigue cracks. Runway girders and bridge-crane end trucks have fillet welds that deserve a look after years of cycling. Pressure vessel nozzle welds, skirt attachments and lifting lugs are examined when the construction code calls for it. Rail car and heavy equipment repair welds, machinery frames, shafts and gear housings round out the list. None of these is exotic, and MT is the quickest way to prove them clean.
What magnetic particle inspection detects, and what it misses
MT works by magnetizing the part and dusting it with fine ferromagnetic particles. A crack or seam that interrupts the magnetic field creates a leakage field at the surface, and the particles gather there, making a visible line. The method finds cracks, laps, seams and lack of fusion that open to the surface or lie just below it, and it does so with high sensitivity and a result the technician can see directly.
The limits are as important as the strengths. The part must be ferromagnetic, which means carbon steel and most low-alloy steels, but not austenitic stainless steel, aluminum, copper or titanium. For those materials, liquid penetrant testing is the surface method, and our Spokane PT page explains it. Deep internal flaws are beyond MT, and so is wall thinning from corrosion, which needs ultrasonic testing. A crack lies in one direction, and the field must cross it at a reasonable angle to make it visible, so each area is magnetized twice, in directions roughly perpendicular to each other. Paint, scale and grease reduce sensitivity, and thick coatings may need removal.
Codes and acceptance criteria for MT work in Spokane
ASME Section V, Article 7, sets the method requirements: the yoke or other magnetizing means, the particle type, the field strength check, the examination procedure content and the evaluation of indications. The acceptance rules come from the construction code. For pressure vessels built to ASME Section VIII Division 1, Mandatory Appendix 6 gives the methods and acceptance standards, and ASME B31.3 process piping refers to its own acceptance table. Structural steel built to AWS D1.1 uses the code's visual and magnetic particle criteria, and bridges built to AWS D1.5 have their own provisions. ASTM E709 is the guide behind many procedures, and ASTM E1444 is the practice commonly invoked by purchase specifications.
Acceptance is never the technician's opinion. A linear indication of a stated length at a stated location is compared with the table that governs the weld, and the report records the table, the measurement and the result. When a specification is silent, the owner or engineer must supply the criterion before the job starts. A good scope names the code edition, the examination extent, whether surface preparation is by others and who dispositions a rejected indication.
Washington pressure equipment oversight and the MT record
Washington's Department of Labor and Industries administers the state boiler and unfired pressure vessel program, including permits and inspections, and it took over Spokane's city program on July 1, 2026. Repairs and alterations to pressure equipment follow the National Board Inspection Code, and weld repairs often require a documented surface examination of the finished weld. A clean MT report is part of the evidence that a repair was made properly, and it travels with the owner's records.
Lifting equipment has its own world. Crane components fall under owner maintenance programs and often under OSHA expectations for inspection of lifting devices, which is why Spokane plants schedule crane hook examination into annual shutdowns. The employer, not Atlantis, decides when and how often an MT examination is required. We perform it, report it and flag anything that needs the owner's engineer or the code inspector.
How the technique is applied
Most field MT uses an electromagnetic yoke. A two-pole yoke placed across a weld creates a field between its legs, and the technician sprays or dusts particles while the yoke is energized. An AC yoke must show a lifting power of at least 10 pounds at the largest pole spacing used, while a direct-current or permanent-magnet yoke must show at least 40 pounds, and the technician verifies this with a test weight rather than assuming it. Particles come in several forms: dry colored powder works well on rough weld surfaces and hot parts, wet visible particles in a spray can give more sensitivity, and fluorescent wet particles used with ultraviolet light give the highest sensitivity of all.
Fluorescent work needs a darkened area and a black light of specified intensity, so it is easiest in a shop or under a tent. Prods, where specified, pass current through the part itself and suit large castings and welds, but they require care to avoid arc burns on finished surfaces. After examination the technician cleans the part, and when residual magnetism would interfere with later welding, machining or bearing service, the part is demagnetized and the remaining field checked with a gauss meter. Cracks found are marked and photographed for the report.
Common problems found on Spokane steel
A few patterns repeat. Fatigue cracks start at the toes of fillet welds that attach lugs, brackets and stiffeners to girders, and they grow in a direction perpendicular to the main stress. Hooks crack at the throat and the shank threads. Pins and shafts crack at keyways, shoulders and fillet radii. Repair welds made without enough preheat show hydrogen cracks in the heat-affected zone, sometimes hours after the weld cooled. Heavy castings carry shrinkage lines and hot tears from the foundry. Knowing where to look is as much a part of the work as knowing how to magnetize, and the technician plans the yoke positions around those spots rather than sweeping at random.
Who performs and reviews the MT work
Examinations are done by technicians qualified under the Atlantis written practice, which follows ASNT SNT-TC-1A. A Level II technician sets up the equipment, performs the examination and interprets indications, while an ASNT Level III approves the written procedure and reviews the reports. Anoop Rayavarapu, ASNT NDT Level III in UT, RT, MT, PT and VT, leads that review. Atlantis is certified to ISO 9001 and ISO 14001. If your contract requires a specific qualification scheme, state it in the request. For procedure writing or a review of your own written practice, see Level III consulting.
What the Spokane MT report contains
The report names the component or weld by tag or drawing number, the procedure and revision, and the surface condition at the time of examination. It records the magnetizing method and equipment, including the yoke's lifting power check or the current used, the particle type and color, the lighting measurement for fluorescent work, and the directions of magnetization. Each indication is described by location, orientation and length, then compared with the acceptance criteria, with the accept or reject decision stated plainly. Sketches or photographs help the engineer find the exact spot. The technician's name, qualification level and the date close the record. Where an area could not be examined, such as a weld too close to a wall for the yoke legs, the limitation is listed.
Planning a magnetic particle job in Spokane
Spokane's climate is dry and cold in winter and hot in summer, and neither extreme is neutral for MT. Steel at freezing temperature is fine for the method, but wet particle carriers thicken, aerosol cans lose pressure and gloved hands miss detail, so winter jobs often move indoors or use a heated enclosure. In July the problem is the reverse: surfaces in direct sun can become too hot for wet particles, which dry too fast, and dry powder or a shaded work area is the practical answer. Winds in open yards also blow dry powder away.
Fluorescent examination needs the ambient white light kept low, so jobs in daylight yards need a tent or a night shift scheduled with the site. Access, isolation and surface preparation are the usual planning items. Welds must be cleaned of slag and heavy paint, and scaffolds or lifts must reach crane girders and tank attachments safely. Plant safety orientation and badging take time at the larger sites, and because Atlantis has no office in Spokane, technicians are mobilized for the agreed scope and the travel is part of the plan.
MT compared with PT and UT for a Spokane job
Pick MT for surface cracks in carbon and low-alloy steel, where speed and sensitivity matter. Pick penetrant when the material is aluminum or stainless, and see the Spokane PT page. Pick ultrasonic testing when the question is wall loss or internal weld quality, and read the Spokane UT page. A typical fabrication job might use UT on the groove welds and MT on the fillets and attachments, with each result reported against the same code. The national magnetic particle testing page, the complete MT guide and the MT versus PT comparison carry the general detail, and the Washington overview is on the Washington inspection services page.
Training your own MT technicians
Shops that run MT every week often train their own staff. Our MT Level 1 training and MT Level 2 training teach the physics, yoke practice and indication interpretation, and the MT training overview explains the format. Your employer certifies the technician under its written practice, and the Spokane NDT training page describes how delivery works for a Spokane team.
Frequently asked questions
Can magnetic particle inspection be used on stainless steel or aluminum in Spokane?
No. MT only works on ferromagnetic materials such as carbon and low-alloy steel. For austenitic stainless steel and aluminum, liquid penetrant testing is the usual surface method, and Atlantis can perform that too.
What yoke strength is required for field MT?
ASME Section V, Article 7 expects an AC yoke to lift at least 10 pounds at the maximum pole spacing used, and a DC or permanent-magnet yoke at least 40 pounds. The technician checks this with a test weight.
Can you inspect crane hooks and lifting beams at my Spokane site?
Yes. Technicians travel to your plant and examine hooks, beams, pins and welds for surface cracks, then report indications and acceptance decisions. The employer sets the inspection interval and decides on any repair.
Do you use wet fluorescent particles or dry powder?
Either, depending on the job. Dry powder suits rough or hot surfaces, visible wet particles give better sensitivity, and fluorescent wet particles under ultraviolet light give the highest sensitivity in a darkened area. The procedure states the choice.
Does the part need to be demagnetized after inspection?
Only when leftover magnetism would interfere with later welding, machining or bearing service, or when the specification asks for it. The technician demagnetizes and checks the residual field with a gauss meter.
Which code decides whether a crack indication is acceptable?
The construction code or owner specification, not the technician. ASME Section VIII Appendix 6, ASME B31.3, AWS D1.1 and AWS D1.5 each have their own criteria, and the report quotes the one that applies.
How cold is too cold for MT in the Spokane winter?
The method itself works on cold steel, but wet carriers thicken and aerosol cans weaken in the cold. Many jobs move indoors or use a heated enclosure, and the procedure states the temperature limits for the materials used.
Does Atlantis have an office in Spokane?
No. Atlantis has no office in the city. Technicians are mobilized to your site for the agreed scope, and travel is planned into the job. Use the quote request to describe what needs inspecting.
Can my staff learn MT and be certified by my company?
Yes. Level 1 and Level 2 courses are available, and your company certifies each person under its written practice following SNT-TC-1A. Atlantis can also review or help write that written practice if needed.
Inspection and training around Spokane
- Ultrasonic testing (UT) in Spokane
- Liquid penetrant testing (PT) in Spokane
- Magnetic particle inspection services
- NDT inspection services in Washington
MT by industry for Spokane: Mining & Minerals · Pulp & Paper · Wind Energy.
MT by job: Magnetic particle weld inspection · Magnetic particle inspection of lifting equipment · Magnetic particle inspection of castings and forgings · Magnetic particle inspection of structural steel and bridges.
Training your own technicians: MT Level 1 training · MT Level 2 training · NDT training for Spokane technicians.
Request an MT inspection quote for Spokane
Send the component and material, the quantity, the code or specification and the site address. We reply within one business day with the scope, the mobilization plan and a quote. Request a quote for magnetic particle inspection in Spokane.
Need magnetic particle testing (MT) done, or learned?
Atlantis provides magnetic particle testing (MT) as an inspection service, trains technicians in it, and lets teams practise it on the Practical NDT simulator.