Magnetic Particle Inspection (MT) in Shreveport, Louisiana

Magnetic particle inspection (MPI, also called mag particle testing) finds surface cracks and other surface-breaking flaws in carbon and low-alloy steel, and Atlantis NDT carries it out at industrial sites in the Shreveport and Bossier City area. Technicians are mobilized to your plant, terminal, yard or shop with yokes, particles, a light meter and field indicators, and report indications against the code you name. Typical targets are weld toes, lugs, crane parts, nozzle attachments and repair excavations. Ask for a magnetic particle quote; a reply comes within one business day.

Where magnetic particle inspection is used around Shreveport

Steel dominates the Shreveport industrial landscape. The city has long been a center for petroleum, natural gas, chemicals and iron and steel products, and the Port of Caddo-Bossier at the head of the Red River navigation handles bulk and industrial cargo in a large industrial park. Gas gathering and compression sites supporting the Haynesville play, tank terminals, rail-served fabrication shops and the maintenance operations around Barksdale Air Force Base all weld, lift and repair carbon steel.

Mag particle jobs that come up in this area:

How the method works, and what it cannot see

The technician magnetizes the part. A crack or similar discontinuity that interrupts the magnetic field causes flux to leak from the surface, and iron particles dusted or sprayed on the part gather there, forming a visible line that outlines the flaw. The method is fast, sensitive to tight cracks that penetrant testing might miss under paint residue or smeared metal, and does not demand a perfectly clean surface.

The limits are firm. The material must be ferromagnetic: carbon steel and most low-alloy steels respond, while austenitic stainless steel, aluminum, copper alloys and brass do not. Only surface and slightly subsurface discontinuities are detected, and sensitivity drops quickly with depth. The method says nothing about wall thickness or deep internal flaws. Flaws are only revealed when they lie across the magnetic field, which is why the field direction is the core technical decision. A crack running parallel to the flux lines can be missed entirely, so a second pass at roughly ninety degrees to the first is required. Thick coatings reduce sensitivity and may need to be removed or demonstrated acceptable.

Codes and acceptance criteria that apply

ASME Section V Article 7 sets the technique requirements, and ASTM E709 is the guide for the method with ASTM E1444 as the practice. Acceptance depends on the construction code. ASME Section VIII Division 1 Appendix 6 defines MT methods and acceptance for vessels, ASME B31.3 paragraph 344.3 and Table 341.3.2 cover process piping, and AWS D1.1 addresses structural steel welds. For in-service work, API 510, 570 and 653 place decisions with the owner's authorized inspector; Atlantis performs the examination and reports the indications that inspector evaluates.

Louisiana adds a layer. The Office of State Fire Marshal's Boiler Inspection Section administers the state's boiler and pressure vessel rules and adopts the ASME Code as the state's construction code, with inspection done by the state or by licensed insurers' inspectors holding a National Board commission. Repairs to jurisdictional vessels follow the National Board Inspection Code. Plants subject to OSHA's process safety management standard in 29 CFR 1910.119 also expect mechanical integrity records that tie to recognized good engineering practice. We write the report so it supports whichever record trail applies.

Technique: yokes, particles and field indicators

For most field work we use an electromagnetic yoke. The Article 7 requirement is that an AC yoke lift at least ten pounds at the pole spacing used, and a DC or permanent-magnet yoke at least forty pounds. We verify that with a test weight before use. Dry visible powder suits warm, rough surfaces such as weld metal; wet visible or fluorescent particles give the highest sensitivity on smooth parts and are viewed under UV-A light in a darkened area, with the intensity and ambient light checked by meter. Contrast paint provides a background when visible particles are used on dark surfaces.

Technicians verify field strength and direction with a pie gauge or a shim indicator, apply the particles while the field is on, and examine in two directions. For critical welds, or on thick sections, prods or a coil may be specified. Afterward, residual magnetism is checked and the part is demagnetized when it would interfere with later welding, machining or service, for example in bearing seats or near instruments. Read the complete guide to magnetic particle testing or the Article 7 explainer for more on the requirements.

Surface condition and preparation

Magnetic particle inspection is forgiving of surface condition compared with penetrant work, but not unlimited. Weld spatter, heavy scale and loose paint lift the yoke legs off the metal and hold particles in false indications, so the area is wire-brushed or ground to bare, clean metal where the procedure requires. Oil and grease prevent particles from moving, so degreasing comes first on equipment that has been in service. Fluorescent work needs especially clean surfaces because contamination fluoresces and hides real indications. We note the surface condition in the report so that a clean result is understood in its context.

Who does the work, and under what authority

Atlantis technicians are qualified under a written practice based on ASNT SNT-TC-1A. Level II technicians set up and calibrate the equipment, perform the examination and interpret indications; an ASNT Level III approves the procedure and reviews the report. Because SNT-TC-1A is employer-based, the company that employs the technician certifies them, which is why we make the written practice available for review. Atlantis has no office in Shreveport. Technicians are mobilized to your site, and we plan travel, orientation and access with you ahead of the work. Our founder, Anoop Rayavarapu, is an ASNT NDT Level III in UT, RT, MT, PT and VT, and procedure approval sits with Level III oversight. For a customer procedure review, see Level III consulting.

What the magnetic particle report records

The report names the component and its location, the procedure and revision, the code and acceptance criteria, and the technique used: yoke type, particle type, wet or dry, color, and the directions examined. It records the lifting-power check, the light meter reading for fluorescent work, surface condition and temperature, and the examination date. The technician and certification level are listed.

Every recordable indication appears with its position, orientation and length, plus a sketch or photograph where useful, and a clear accept or reject against the named criteria. If a flaw is ground out, the follow-up examination of the excavation is recorded the same way. The result is a document that stands up when an authorized inspector, an insurer or a customer auditor asks how a repair was verified.

Common problems we watch for on mag particle jobs

Most poor magnetic particle results trace back to a handful of causes, and a careful technician checks for each one before accepting a clean result. Poor contact between yoke legs and a rough or painted weld reduces flux in the part, so surface condition is inspected first. A yoke used at the wrong pole spacing delivers less field than the lift test assumed. Particles applied after the field is switched off, or applied too heavily, either wash off the indication or bury it. Non-relevant indications, such as those at a sharp change of section or the edge of a magnetic writing mark, are a common source of confusion and have to be separated from true flaws by re-examination, often after light dressing of the surface.

The same discipline applies to repair work. When a crack is ground out, the excavation is re-examined before welding to prove the flaw is gone, and again after welding and any required post-weld heat treatment, since some cracks do not appear until the weld has cooled. Recording each step gives the owner and the authorized inspector a clear chain from defect to repair to final acceptance.

Planning a magnetic particle job in Shreveport

Weather is a real factor on outdoor steel. Midsummer heat can push a shell past the temperature where wet particles dry too fast and carrier liquid evaporates, and humid air complicates surface cleaning and drying of particle suspensions. Spring storms and winter cold bring their own constraints, so a covered work area or schedule flexibility helps. For fluorescent work, UV-A examination needs darkness or a tent, which can be difficult in full sun.

Tell us the base metal, coating and weld type, the code, and how much of each weld needs examination. Provide access, power if needed and any hot work or confined space permits. Plant orientation and badging are common at gas and process facilities in the area, and port-side sites add their own access routines. Early notice lets us line up the right equipment, which is especially useful for turnaround and shutdown windows when crews are scarce.

MT, PT or UT for your Shreveport job

Magnetic particle inspection is the first choice for surface cracks in carbon steel welds. If the part is stainless or aluminum, or the surface is non-magnetic, use liquid penetrant testing in Shreveport. If you need wall thickness, corrosion rate or a volumetric examination of a weld, ultrasonic testing in Shreveport is the fit. Repair packages often combine methods. Read MT versus PT compared for a quick decision guide, or see the national magnetic particle testing page and the Louisiana inspection services hub.

Training your own MT technicians

For in-house capability, Atlantis offers MT Level 1 training and MT Level 2 training. Your company certifies its own personnel under its written practice. Local readers can also look at NDT training for Shreveport, and check SNT-TC-1A eligibility to see what experience hours apply.

Frequently asked questions

What materials can magnetic particle inspection be used on?

Ferromagnetic materials only, which in practice means carbon steel and most alloy steels. It does not work on austenitic stainless steel, aluminum or copper alloys, which are not attracted to a magnet. For those materials, liquid penetrant testing is the usual surface method.

Is mag particle testing able to find subsurface cracks?

It can reveal flaws just under the surface, but sensitivity falls quickly with depth. Deep internal flaws are outside the method. If you need to find internal weld flaws or measure remaining wall, ultrasonic testing is the appropriate method.

Why are two directions of magnetization required?

A flaw shows only when it crosses the magnetic field. A crack parallel to the field lines can be missed, so the part is examined with the field in two directions at roughly right angles. That is how the code makes sure cracks in any orientation are caught.

Do you use wet or dry magnetic particles?

We choose by the job. Dry visible powder suits rough, warm weld surfaces. Wet particles, visible or fluorescent, give higher sensitivity on smooth surfaces and are common for critical welds. The procedure states the choice and the code or owner specification can require one.

Does paint or coating need to be removed before MT?

Thin, tight coatings can sometimes remain if the procedure demonstrates that sensitivity is still adequate. Thick or flaking coatings usually have to be removed. We confirm the limit with a demonstration on a representative sample before examining the real part.

When is demagnetization needed after inspection?

When residual magnetism could interfere with later welding, machining, instruments or service, such as arc blow during welding or particles clinging to bearing surfaces. The technician checks the residual field and demagnetizes if it exceeds the limit set in the procedure.

Can you do magnetic particle inspection at night or during a shutdown?

We can schedule technicians around your outage windows. Fluorescent examination actually benefits from darkness. Tell us your shutdown schedule early so that equipment and personnel are lined up. We do not promise a specific arrival time before the scope is agreed.

Does Atlantis have a Shreveport office or lab?

No. Atlantis has offices in Houston and Hyderabad, and technicians travel to your Shreveport or Bossier City site. Orientation, badging, power and access are planned with you before the work starts.

Who certifies Atlantis technicians for MT?

Under ASNT SNT-TC-1A the employer certifies its own personnel. Atlantis qualifies technicians under its written practice, with Level II performing and interpreting and an ASNT Level III approving procedures and reviewing reports. We can share that written practice for audit.

Inspection and training around Shreveport

MT by industry for Shreveport: Pipeline · Oilfield & Drilling · Pulp & Paper.

MT by job: Magnetic particle weld inspection · Magnetic particle inspection of lifting equipment · Magnetic particle inspection of castings and forgings · Magnetic particle inspection of structural steel and bridges.

Training your own technicians: MT Level 1 training · MT Level 2 training · NDT training for Shreveport technicians.

Request an MT inspection quote for Shreveport

Send the component and material, the quantity, the code or specification and the site address. We reply within one business day with the scope, the mobilization plan and a quote. Request a quote for magnetic particle inspection in Shreveport.

Need magnetic particle testing (MT) done, or learned?

Atlantis provides magnetic particle testing (MT) as an inspection service, trains technicians in it, and lets teams practise it on the Practical NDT simulator.