{"slug":"/standards/asme-b31-1-acceptance-criteria","title":"ASME B31.1 Acceptance Criteria for Power Piping Welds","description":"B31.1 para. 136.4 acceptance standards for visual, MT, PT, RT and UT, the Table 136.4 mandatory minimum examinations by service, and how they differ from B31.3.","h1":"Power Piping Weld Acceptance Under ASME B31.1 Para. 136.4: Visual, MT, PT, RT and UT","answer":"ASME B31.1 states weld acceptance in para. 136.4, method by method: visual in 136.4.2, magnetic particle in 136.4.3, penetrant in 136.4.4, radiography in 136.4.5 and ultrasonics in 136.4.6. Table 136.4 sets which welds need more than visual examination, by weld type, size, thickness and service temperature and pressure. Every weld is examined visually, and an external crack is never acceptable.","expansion":"Visual acceptance under 136.4.2 rejects surface cracks, surface lack of fusion, undercut deeper than 1/32 in. (1.0 mm) or encroaching on the minimum required wall, any surface undercut on a longitudinal butt weld, reinforcement beyond Table 127.4.2, incomplete penetration where the inside surface is readily accessible, other linear indications over 3/16 in. (5.0 mm), and surface porosity beyond stated size and spacing limits. Penetrant acceptance adds an area rule the Section VIII appendices do not have: ten or more rounded indications in any 6 sq in. of surface reject the weld. A weld that Table 136.4 does not send to RT, UT, MT or PT is acceptable once it passes visual examination and the pressure test. The table is a floor, and the engineering design can require more. B31.3 process piping is organised differently, around fluid service, random examination and Table 341.3.2.","source":"ASME B31.1 Power Piping (2016 edition): para. 136.1, 136.4.1, 136.4.2 (visual), 136.4.3 (magnetic particle), 136.4.4 (liquid penetrant), 136.4.5 (radiography), 136.4.6 (ultrasonic), Table 136.4 with its general notes and notes, Table 127.4.2, para. 137; ASME BPVC Section V Articles 2, 4, 6, 7 and 9; ASME BPVC Section I for boiler external piping administration; ASME B31.3 para. 341.3.4 and Table 341.3.2 for contrast. If the contract invokes a later edition, confirm the paragraph and table numbers as well as the values, because ASME revises and renumbers tables between editions. The 2022 edition numbers the minimum-examination table Table 136.4.1-1 and adds Table 136.4.1-2; the 2024 edition is current.","table":{"caption":"B31.1 visual and penetrant acceptance limits, para. 136.4 (2016 edition)","columns":["Imperfection","Rejected when","Paragraph","Practical note"],"rows":[["External surface crack","Present at any size","136.4.2","No length allowance"],["Undercut","Deeper than 1/32 in. (1.0 mm), or encroaching on minimum required wall thickness","136.4.2","Record the measured depth"],["Undercut on longitudinal butt welds","Any surface undercut","136.4.2","Stricter than the girth-weld rule"],["Weld reinforcement","Exceeds Table 127.4.2","136.4.2","Read the table for the wall thickness"],["Surface lack of fusion","Present at any size","136.4.2",""],["Incomplete penetration","Present, where the inside surface is readily accessible","136.4.2","Otherwise left to volumetric examination"],["Other linear indications (visual)","Longer than 3/16 in. (5.0 mm)","136.4.2",""],["Surface porosity (visual)","Rounded indication over 3/16 in. (5.0 mm), or four or more separated by 1/16 in. (2.0 mm) or less","136.4.2",""],["Penetrant: cracks and linear indications","Any","136.4.4","MT acceptance has its own subparagraph, 136.4.3"],["Penetrant: rounded indications","Over 3/16 in. (5.0 mm); four or more in a line 1/16 in. (2.0 mm) or less apart edge to edge; ten or more in any 6 sq in. (3 870 mm2) with major dimension no more than 6 in. (150 mm)","136.4.4","The area rule has no counterpart in Section VIII Appendices 6 and 8"]],"note":"Radiographic (136.4.5) and ultrasonic (136.4.6) acceptance limits are in their own subparagraphs; read them in the edition invoked. Values are in U.S. customary units with the SI equivalents B31.1 prints."},"sections":[{"heading":"How para. 136.4 is put together","paragraphs":["B31.1 has no single acceptance table covering every method. Para. 136.4.1 sets out the arrangement: the types and extent of mandatory examination for pressure welds come from Table 136.4, each method has its own subparagraph of acceptance standards, and a weld that the table does not send to radiography, ultrasonics, magnetic particle or penetrant examination is acceptable if it passes visual examination under 136.4.2 and the pressure test under para. 137. That last provision is easy to overlook: for a large share of welds in lower-severity service, visual examination is the whole of the code's nondestructive examination requirement.","The general paragraph also deals with timing. For welds in P-No. 3, 4, 5A, 5B and 15E materials, the chromium-molybdenum family that includes Grade 22 and Grade 91, the nondestructive examination is performed after postweld heat treatment unless the engineering design directs otherwise; for other materials it may be done before or after. A procedure that schedules magnetic particle examination on a Grade 91 weld before heat treatment and then accepts the result has not met the code, however clean the indication record looks. Our [B31.1 code page](/standards/asme-b31-1) covers the design, heat treatment and pressure-test side of the code."]},{"heading":"Which B31.1 edition the numbers come from","paragraphs":["The paragraph and table numbers on this page follow the 2016 edition, and the code has been reissued in 2018, 2020, 2022 and 2024 since then. The numbering has moved: the contents of the 2022 edition list the mandatory minimum examination table as Table 136.4.1-1, Mandatory Minimum Nondestructive Examinations for Pressure Welds or Welds to Pressure-Retaining Components, and add Table 136.4.1-2, Weld Imperfections Indicated by Various Types of Examination. A procedure written for current work should cite those designations rather than the older Table 136.4.","The 2024 edition is the current one. A published summary of its changes lists new mandatory appendices on quality management and on documentation for non-boiler external covered piping systems and rewritten rules for bolted flanged connections and for rerating, and it does not list changes to para. 136; that summary is no substitute for reading the edition the contract names. Regulations can also hold an older edition in place. The Coast Guard's marine engineering rules call for piping nondestructive examination in accordance with Table 136.4 of B31.1, so work under 46 CFR 56.95-10 carries the older table reference and the edition that regulation incorporates. Where a jurisdiction adopts B31.1 by reference, confirm the adopted edition before quoting a cell."]},{"heading":"Mandatory minimum examination: reading Table 136.4","paragraphs":["Table 136.4 has three service columns and three weld-type rows. The columns, in the edition we checked, are temperatures over 750°F (400°C) at all pressures; temperatures from 350°F to 750°F (175°C to 400°C) inclusive with pressures over 1,025 psig; and all other service. The rows are butt welds (girth and longitudinal), welded branch connections, and fillet, socket, attachment and seal welds. The general notes say that every weld receives visual examination in addition to the listed examination, and that the acceptance standards are those of 136.4.2 through 136.4.6.","The cells turn on size and thickness. In the highest-temperature column, butt welds above NPS 2 (DN 50) are examined by radiography or ultrasonics; the intermediate column applies that examination only where the wall is over 3/4 in. (19.0 mm) and otherwise asks for visual examination. Branch connections follow the same pattern with NPS 4 (DN 100) as the dividing size, with magnetic particle or penetrant examination for the smaller branches where the column calls for more than visual. In the highest-temperature column, fillet, socket, attachment and seal welds also receive magnetic particle or penetrant examination; in the all-others column the minimum for every weld type is visual examination. Read the exact cell for the column that applies rather than relying on a summary, because the wording of the size and thickness conditions has been revised over time.","The notes matter as much as the cells. Butt weld thickness is taken as the thicker of the two abutting ends after weld preparation; radiography may be substituted for a required magnetic particle or penetrant examination; volumetric examination of a branch is done before any non-integral reinforcement is added; surface examination may be accepted in place of a required volumetric examination of a welded branch connection, under the conditions that note sets; and fillet welds of 1/4 in. (6 mm) throat or less used for non-pressure attachments are exempt from surface examination. Longitudinal and spiral welds in pipe intended for service in the creep range need 100 percent volumetric examination. Above all, the table is a mandatory minimum: the engineering design can require more, and when it does, the larger extent governs."]},{"heading":"Placing a line in its Table 136.4 column","paragraphs":["Every Table 136.4 decision starts with the service column, and the boundaries are easy to misread. A main steam line whose design basis is above 750°F (400°C) belongs in the first column whatever its pressure. A feedwater line at 480°F and 2,600 psig falls in the second column, because it lies between 350°F and 750°F inclusive and above 1,025 psig. The same line at 900 psig drops to the all-others column, and so does any line at 300°F. A line at exactly 750°F with a pressure over 1,025 psig is in the second column, because that band includes 750°F; at 760°F it moves to the first.","Write the temperature and pressure basis used for each line class into the inspection plan. An uprate, a change in operating conditions or a corrected design figure can move welds into a column that calls for heavier examination, and welds already accepted on visual examination alone may then need volumetric or surface examination before the change takes effect."]},{"heading":"Visual acceptance in 136.4.2","paragraphs":["Visual examination follows Section V Article 9 for technique, and B31.1 recognises in-process visual examination during fabrication and erection to confirm that the design and the welding procedure are being followed. The acceptance list itself is short and absolute. External surface cracks, surface lack of fusion and reinforcement beyond Table 127.4.2 are rejected. Undercut is rejected if it is deeper than 1/32 in. (1.0 mm) or encroaches on the minimum required wall thickness, and on longitudinal butt welds any surface undercut is unacceptable, a stricter rule than many inspectors expect.","Incomplete penetration is a visual rejection only where the inside surface is readily accessible, which on most pipe means it is caught by volumetric examination or not at all. Other linear indications longer than 3/16 in. (5.0 mm) are rejected, and surface porosity is rejected when a rounded indication exceeds 3/16 in. (5.0 mm) or four or more lie with 1/16 in. (2.0 mm) or less between them. Because many B31.1 welds are accepted on visual examination alone, the visual inspector's measurements, undercut depth with a gauge, reinforcement height against the table and the length of any linear feature, are the acceptance record, and they should be written down as numbers. Our [visual testing page](/visual-testing) describes how those examinations are carried out on site."]},{"heading":"Magnetic particle and penetrant acceptance (136.4.3 and 136.4.4)","paragraphs":["Surface examination is required by Table 136.4 for some welds and may be replaced by radiography under the table's notes. Penetrant acceptance under 136.4.4 rejects any crack or linear indication, any rounded indication larger than 3/16 in. (5.0 mm), four or more rounded indications in a line separated by 1/16 in. (2.0 mm) or less edge to edge, and ten or more rounded indications in any 6 sq in. (3 870 mm2) of surface, where the major dimension of that area is no more than 6 in. (150 mm). Magnetic particle acceptance has its own subparagraph, 136.4.3, and the procedure should cite that paragraph for MT rather than borrowing the penetrant reference.","The area-density rule is the practical difference from Section VIII Division 1, whose penetrant and magnetic particle appendices contain no ten-in-an-area criterion. A field of fine scattered porosity that passes a vessel examination can fail a B31.1 examination of the same surface, so contractors working across both codes should not reuse one acceptance clause. The SI equivalents differ as well: B31.1 prints 1/16 in. as 2.0 mm, where the Division 1 appendices use 1.5 mm. Work to the units the contract names, and do not mix conversions from two codes in one report. Technique for both methods is set by Section V; see our pages on [magnetic particle weld inspection](/magnetic-particle-weld-inspection) and [penetrant testing of welds](/penetrant-testing-welds)."]},{"heading":"Radiographic acceptance (136.4.5)","paragraphs":["Where Table 136.4 calls for volumetric examination and radiography is the method chosen, the technique follows Section V Article 2 and the acceptance standards are those of 136.4.5. Like the boiler and vessel codes, B31.1 rejects crack-like indications and incomplete fusion or penetration outright and limits other indications by type, length and grouping in relation to weld thickness, with porosity judged against the rounded-indication standard in Appendix A-250 of Section I, and root concavity rejected where the radiograph shows an abrupt change in density. Read the values from 136.4.5 in the edition invoked; do not take them from Section VIII UW-51 or from B31.3 Table 341.3.2 because the format looks alike.","Table 136.4 leaves the choice between radiography and ultrasonics open in its volumetric cells, so the procedure has to name the method and the matching acceptance subparagraph. A radiograph review starts with the technique record, covering source, exposure arrangement, IQI and density, before the indications, because an acceptable-looking film made with the wrong technique demonstrates nothing. Radiography is outside Atlantis's scope in the United States; ultrasonic testing covers volumetric examination where the code permits it, and our ASNT Level III can review the radiographs and RT procedures of the owner's licensed radiography contractor."]},{"heading":"Ultrasonic acceptance (136.4.6) and UT used in place of RT","paragraphs":["Ultrasonic examination performed to satisfy a volumetric cell of Table 136.4 is carried out to Section V Article 4 and judged to 136.4.6. The review questions are those of any ultrasonic acceptance standard: what reference reflector and level the evaluation is based on, how indications are characterised, how length is measured, and whether the technique recorded enough data for someone else to check the decision. Check also whether the contract or the owner's specification adds requirements for the technique, such as encoded scanning, because the code paragraph sets a minimum, not a ceiling.","On creep-range piping in Grade 91 and similar alloys, the timing rule in 136.4.1 means the ultrasonic examination is done after heat treatment, and the scan plan has to cover the weld volume and heat-affected zone for the actual joint geometry, including counterbore and taper at fittings. Our [ultrasonic weld inspection](/ultrasonic-weld-inspection) service and the [UT acceptance criteria by code](/standards/ut-acceptance-criteria-by-code) guide explain how the technique and the code limits fit together."]},{"heading":"B31.1 against B31.3: same family, different rules","paragraphs":["B31.1 and B31.3 are both ASME pressure piping codes, and many plants contain both. B31.3 organises examination around fluid service, with Normal, Category D, Category M, severe cyclic and high-pressure service, random examination of a percentage of welds, progressive examination when a sample fails, and one acceptance table, Table 341.3.2, listing imperfections against the service categories. B31.1 instead lists mandatory minimum examinations by service temperature and pressure in Table 136.4, and spreads its acceptance standards across method-specific subparagraphs.","The practical consequences are concrete. A B31.3 weld can be accepted as part of a lot whose random sample passed; a B31.1 weld in a cell that requires volumetric examination is examined individually. B31.3's progressive scheme, with additional samples taken when one fails, has no counterpart in Table 136.4. The inspection role differs too: B31.1 para. 136.1 places inspection with an owner's inspector who, as a rule, is not an employee of the manufacturer, fabricator or erector. Our [B31.3 acceptance criteria guide](/standards/asme-b31-3-acceptance-criteria) covers the process piping side."]},{"heading":"Boiler external piping and in-service work","paragraphs":["Boiler external piping sits inside B31.1 for its technical rules, so its welds are examined to Table 136.4 and accepted to para. 136.4, but it is administered under ASME Section I: the Authorized Inspector, the data reports and the piping limits come from the boiler code. Non-boiler external piping has no Authorized Inspector; the owner's inspector under para. 136.1 carries the inspection role. Confusing the two produces records that are technically right and administratively wrong. The boiler side of the boundary is covered in our guide to [Section I weld acceptance criteria](/standards/asme-section-i-acceptance-criteria).","B31.1 acceptance standards are construction standards. Once a power piping system is in service, the owner's programme decides what is examined and when, repairs to boiler external piping are made under the National Board Inspection Code where the jurisdiction requires it, and an indication found in service is evaluated by the owner's engineer rather than rejected automatically against 136.4. Atlantis does not perform fitness-for-service assessments; we size and characterise indications so the engineer has reliable data to work from."]},{"heading":"What reviewers find in B31.1 procedures and reports","paragraphs":["Procedures that cite Section V as the acceptance standard. Acceptance clauses copied from B31.3 Table 341.3.2 or from the Section VIII appendices, which carry different limits and, for the surface methods, no area rule. Examination scheduled before heat treatment on P-No. 5A, 5B or 15E welds. Undercut on longitudinal seams judged against the 1/32 in. depth limit instead of being rejected. Butt weld thickness taken from the thinner end when the table note uses the thicker end after preparation. Table 136.4 treated as the full extent when the engineering design asks for more. Visual reports that say accept without recording undercut depth or reinforcement height.","A defensible B31.1 report names the edition, the Table 136.4 column and row that set the examination, the subparagraph of 136.4 used for acceptance, the method and technique, each relevant indication with location and size, and the decision. For boiler external piping it also identifies the Authorized Inspector's acceptance step. Report templates in [Atlantis ERP](/erp/apps/ndt-reports) can be set up to carry the acceptance subparagraph on every report, so the reference travels with the result."]},{"heading":"Where Atlantis fits","paragraphs":["Our ASNT NDT Level III prepares B31.1 examination procedures with the acceptance subparagraph and edition written in, qualifies and demonstrates ultrasonic techniques for heavy-wall and alloy piping, and reviews contractor reports and radiographs against para. 136.4 before turnover. See [procedure qualification and demonstration](/consulting/ndt-procedure-qualification-demonstration) and [NDT Level III consulting](/consulting/ndt-consulting-level-iii).","In the United States, Atlantis technicians carry out ultrasonic, magnetic particle, penetrant and visual examination of power piping at the client's site; see [NDT for power generation](/ndt-for-power-generation). Inspectors learning to apply para. 136.4 can use [magnetic particle training](/magnetic-particle-testing-training) and [penetrant training](/penetrant-testing-training), and the [acceptance criteria by code hub](/standards/ndt-acceptance-criteria-by-code) shows where the other construction codes keep their limits."]}],"facets":[{"q":"Where are the weld acceptance criteria in ASME B31.1?","a":"In para. 136.4. Visual acceptance is in 136.4.2, magnetic particle in 136.4.3, liquid penetrant in 136.4.4, radiography in 136.4.5 and ultrasonics in 136.4.6. Table 136.4 sets which welds need examination beyond visual, by weld type, size, thickness and service temperature and pressure. ASME Section V supplies the technique for each method but no acceptance values."},{"q":"What undercut does ASME B31.1 allow?","a":"Under 136.4.2, undercut is rejected if it is deeper than 1/32 in. (1.0 mm) or if it encroaches on the minimum required wall thickness. On longitudinal butt welds any surface undercut is unacceptable. Measure the depth with a suitable gauge and record the value, because many B31.1 welds are accepted on visual examination alone and the measurement is the acceptance evidence."},{"q":"Which B31.1 welds need radiography or ultrasonic examination?","a":"Table 136.4 decides, by service band and weld type. In the highest-temperature column, butt welds above NPS 2 are examined by radiography or ultrasonics; the intermediate column adds a wall-thickness condition, and branch connections use NPS 4 as their dividing size. In the all-others column visual examination is the minimum. Read the exact cell in your edition, and remember the engineering design can require more."},{"q":"What are the B31.1 penetrant acceptance criteria?","a":"Para. 136.4.4 rejects any crack or linear indication, any rounded indication larger than 3/16 in. (5.0 mm), four or more rounded indications in a line separated by 1/16 in. (2.0 mm) or less edge to edge, and ten or more rounded indications in any 6 sq in. of surface whose major dimension is no more than 6 in. Magnetic particle acceptance has its own subparagraph, 136.4.3."},{"q":"Are B31.1 acceptance criteria the same as B31.3?","a":"No. B31.3 sets examination by fluid service, with random sampling and progressive examination, and judges welds against Table 341.3.2. B31.1 sets mandatory minimum examination by service temperature and pressure in Table 136.4 and states acceptance method by method in para. 136.4. A clause written for one code should not be reused on the other, even where some numbers coincide."},{"q":"Can a B31.1 weld be accepted on visual examination alone?","a":"Yes, where Table 136.4 does not require radiography, ultrasonics, magnetic particle or penetrant examination. Para. 136.4.1 accepts such a weld when it passes visual examination under 136.4.2 and the pressure test under para. 137, unless the engineering design or the owner's specification requires more. For those welds the visual record is the whole of the acceptance evidence."}],"faq":[{"q":"Where are the weld acceptance criteria in ASME B31.1?","a":"In para. 136.4. Visual acceptance is in 136.4.2, magnetic particle in 136.4.3, liquid penetrant in 136.4.4, radiography in 136.4.5 and ultrasonics in 136.4.6. Table 136.4 sets which welds need examination beyond visual, by weld type, size, thickness and service temperature and pressure. ASME Section V supplies the technique for each method but no acceptance values."},{"q":"What undercut does ASME B31.1 allow?","a":"Under 136.4.2, undercut is rejected if it is deeper than 1/32 in. (1.0 mm) or if it encroaches on the minimum required wall thickness. On longitudinal butt welds any surface undercut is unacceptable. Measure the depth with a suitable gauge and record the value, because many B31.1 welds are accepted on visual examination alone and the measurement is the acceptance evidence."},{"q":"Which B31.1 welds need radiography or ultrasonic examination?","a":"Table 136.4 decides, by service band and weld type. In the highest-temperature column, butt welds above NPS 2 are examined by radiography or ultrasonics; the intermediate column adds a wall-thickness condition, and branch connections use NPS 4 as their dividing size. In the all-others column visual examination is the minimum. Read the exact cell in your edition, and remember the engineering design can require more."},{"q":"What are the B31.1 penetrant acceptance criteria?","a":"Para. 136.4.4 rejects any crack or linear indication, any rounded indication larger than 3/16 in. (5.0 mm), four or more rounded indications in a line separated by 1/16 in. (2.0 mm) or less edge to edge, and ten or more rounded indications in any 6 sq in. of surface whose major dimension is no more than 6 in. Magnetic particle acceptance has its own subparagraph, 136.4.3."},{"q":"Are B31.1 acceptance criteria the same as B31.3?","a":"No. B31.3 sets examination by fluid service, with random sampling and progressive examination, and judges welds against Table 341.3.2. B31.1 sets mandatory minimum examination by service temperature and pressure in Table 136.4 and states acceptance method by method in para. 136.4. A clause written for one code should not be reused on the other, even where some numbers coincide."},{"q":"Can a B31.1 weld be accepted on visual examination alone?","a":"Yes, where Table 136.4 does not require radiography, ultrasonics, magnetic particle or penetrant examination. Para. 136.4.1 accepts such a weld when it passes visual examination under 136.4.2 and the pressure test under para. 137, unless the engineering design or the owner's specification requires more. For those welds the visual record is the whole of the acceptance evidence."}]}